SOLID SOLUTION POWDERRS OF TANTALUM-NIOBIUM CARBIDE
Grade |
90:10 |
80:20 |
70:30 |
60:40 |
50:50 |
||
Chemical composition |
Ta |
84.4±1.5 |
71.5±1.5 |
65.6±1.5 |
56.0±1.3 |
46.9±1.3 |
|
Nb |
8.85±1.0 |
21±1.0 |
26.6±1.2 |
35.0±1.3 |
44.3±1.5 |
||
T.C |
6.75±0.3 |
7.3±0.3 |
7.8±0.3 |
8.2±0.3 |
8.8±0.3 |
||
F.C |
≤0.15 |
≤0.15 |
≤0.15 |
≤0.15 |
≤0.15 |
||
Impurities content%,max |
Co |
0.1 |
0.1 |
0.1 |
0.1 |
0.1 |
|
Mo |
0.1 |
0.1 |
0.1 |
0.1 |
0.1 |
||
Si |
0.02 |
0.02 |
0.02 |
0.02 |
0.02 |
||
Fe |
0.15 |
0.15 |
0.15 |
0.15 |
0.15 |
||
Ni |
0.04 |
0.04 |
0.04 |
0.04 |
0.04 |
||
K |
0.008 |
0.008 |
0.008 |
0.008 |
0.008 |
||
Na |
0.008 |
0.008 |
0.008 |
0.008 |
0.008 |
||
Mn |
0.05 |
0.05 |
0.05 |
0.05 |
0.05 |
||
Sn |
0.01 |
0.01 |
0.01 |
0.01 |
0.01 |
||
Ca |
0.01 |
0.01 |
0.01 |
0.01 |
0.01 |
||
Al |
0.015 |
0.015 |
0.015 |
0.015 |
0.015 |
||
N |
0.25 |
0.2 |
0.25 |
0.25 |
0.25 |
||
O |
1 |
0.35 |
0.35 |
0.35 |
0.35 |
0.35 |
|
2 |
0.25 |
0.25 |
0.25 |
0.25 |
0.25 |
||
3 |
0.2 |
0.2 |
0.2 |
0.2 |
0.2 |
||
Ti |
0.2 |
0.3 |
0.3 |
0.3 |
0.3 |
||
W |
0.2 |
0.35 |
0.35 |
0.35 |
0.35 |
||
Cr |
0.1 |
0.1 |
0.1 |
0.1 |
0.1 |
||
Fsss μm |
1 |
1.0-1.2 |
|||||
2 |
1.2-1.5 |
||||||
3 |
1.5-3.5 |
||||||
Application |
For cemented carbide |
CONTACT INFORMATION
Tel:0731-28227700(office)
Tel:0731-26291888(Factory)
E-mail:sarah_zhuzhu@topcarbide.com
OFFICIAL ACCOUNTS
Follow our official public account
ONLINE MESSAGE
Copyright© 2017 Zhuzhou Top Carbide Material Co., Ltd. | 湘ICP备17017431号-1 by:www.300.cnchangsha This site already supports ipv6 access